Swollen O-rings: causes and fixes
Quick answer
At a glance
- Avoid with
- Incompatible oils, fuels, solvents and cleaning chemicals
- Also known as
- O-Ring Swelling, Seal Swelling, Elastomer Swelling
The full explanation
THE FULL EXPLANATION
O-rings are designed to create a reliable seal between two surfaces. However, exposure to certain liquids, chemicals or operating conditions can cause the rubber to swell.
Swelling occurs when the O-ring absorbs substances from its surroundings, increasing its volume and potentially changing its physical properties.
1. Chemical Incompatibility
The most common cause of O-ring swelling is contact with an incompatible liquid or chemical.
For example, EPDM O-rings are generally unsuitable for petroleum-based oils and fuels, while nitrile (NBR) O-rings can swell when exposed to certain solvents.
Choosing the correct rubber material is essential for preventing this problem.
2. Incorrect Lubricants
Some greases and lubricants can react with rubber materials, causing them to swell or soften.
A lubricant that works well with one type of rubber may damage another. Always check compatibility before applying lubricants during installation.
3. Excessive Temperatures
High temperatures can accelerate fluid absorption and chemical degradation.
Even an O-ring that performs well at room temperature may experience excessive swelling when exposed to the same chemical at elevated temperatures.
4. Using the Wrong O-Ring Material
Different rubber materials are designed for different environments.
Common options include:
- Nitrile (NBR): Generally suitable for mineral oils, grease and many petroleum-based fuels.
- FKM (Viton®): Offers excellent resistance to many oils, fuels and chemicals, particularly at higher temperatures.
- EPDM: Suitable for water, steam in appropriately specified grades, and many glycol-based fluids.
- Silicone (VMQ): Offers excellent flexibility across a wide temperature range but has limitations with certain oils, fuels and solvents.
Compatibility depends on the exact chemical, rubber compound and operating temperature.
COMMON MISTAKES
Reusing a swollen O-ring
Even if it appears to return to its original size after drying, its sealing properties may have changed. Replacing it is the safer option.
Assuming all rubber materials are the same
Nitrile, EPDM, FKM and silicone offer different levels of chemical resistance. Choosing the wrong material can result in premature failure.
Ignoring cleaning chemicals
An O-ring may be compatible with its normal operating fluid but unsuitable for the chemicals used during cleaning or maintenance.
Choosing a smaller O-ring to compensate for swelling
Swelling indicates a potential material compatibility problem. Installing a smaller O-ring is not a reliable solution.
Overlooking operating temperatures
Chemical resistance can change significantly at higher temperatures. Always consider both the fluid and the working temperature.
HOW TO FIX A SWOLLEN O-RING
If you've discovered a swollen O-ring, follow these steps:
- Identify the fluid: Determine which oils, fuels, chemicals or lubricants the O-ring has been exposed to.
- Check the material: Establish whether the existing O-ring is nitrile, EPDM, FKM, silicone or another compound.
- Confirm operating conditions: Consider the temperature, pressure and whether the seal is static or moving.
- Choose a compatible replacement: Select an O-ring material suitable for the specific application.
- Check the dimensions: Ensure the replacement has the correct internal diameter and cross-section.
Important: Do not assume FKM (Viton®) is always the best replacement. Although it offers excellent chemical resistance, it is unsuitable for certain applications. Material selection should always be based on the operating conditions.